Silicon Steel Core
Silicon steel core process using core winding machine and material sheet thickness 0.23 mm. Core's shape and dimension is formed by shaft core winding machine such as round core's, rectangular core's and oval core's. Then core's finish using an auto coating machine after heat treatment process.
Application : Silicon steel core's are used in Current Transformer Products (CT)